AZ-1681 Stone adhesive/Epoxy resin for repairing surface cracks in stone slabs

Application:
The product is used to repair irregular fissures—such as micro-cracks (pinholes, "chicken-wire" patterns, or fine, winding cracks)—and uneven areas on the surface of various types of stone. It can serve as a replacement for the following products:
RESIN 5008 (used with catalysts BB25, BX30, or BX40)
RESIN 1006 (used with catalysts BB25, BX30, or BX40)

Price Interview

Price Interview

AZ-1681 Stone adhesive/Epoxy resin for repairing surface cracks in stone slabs

Interview

Select the number of specifications

Please check the product information you want!

Product Detail Applications & Benefits

Mixing ratio: A:B = 4:1

Color: Colorless, transparent liquid.

Viscosity (25°C, mPa•s):

A: 800–1200

B: 300–500

Gel time (25°C, min): 15–25

Curing time (25°C, h): 3–4

Tensile shear strength (MPa): ≥8

Can be used for coating marble surfaces, repairing cracks and voids, and enhancing surface gloss after polishing.

250 kg/set

[Product Advantages]

1. High adhesion and strength; excellent penetration into small cracks;

2. Low odor; poses no health risks to workers;

3. Good resistance to aging and yellowing;

4. Compliant with GB18583 standards and RoHS directives; environmentally friendly.

[Instructions]

1. Slab Preparation

Slabs must be completely dry.

Remove any mud, oil, or other impurities from the slab surface.

2. Adhesive Preparation and Mixing

Mix the adhesive components in an A:B ratio of 4:1 (by weight) until homogeneous.

Use the adhesive within its pot life. The adhesive generates heat during the reaction; do not use it once the pot life has expired. A larger volume of mixed adhesive or a higher ambient temperature will result in a shorter pot life. If preparing a large batch, divide it promptly for use.

Do not swap the caps for components A and B. Keep the containers tightly closed at all times to prevent the ingress of moisture or dust from the air. It is recommended to use wide-mouthed containers for mixing to extend the adhesive's pot life.

3. Adhesive Application

Spread the adhesive evenly over the surface of the slab using a spatula, employing a back-and-forth motion. The recommended application rate is 80–150 g/m².

For cracks in the slabs, work the adhesive in using a back-and-forth motion to ensure complete penetration.

For larger defects (such as embedded soil or debris), remove the foreign material first; then, mix the adhesive with stone dust to perform the repair. Once cured, polish the area and reapply the adhesive. Do not use surface treatment agents that are not epoxy-based, as they may render the surface unsuitable for the application of epoxy adhesive.

4. Curing

The adhesive will reach an initial cure in 2 to 3 hours at room temperature (25 °C); the next processing stage can begin after 24 hours.

If possible, heat the stone (with the adhesive applied) to a temperature between 50 °C and 60 °C, and proceed with polishing after 2 to 3 hours.

Before the adhesive has cured, the stone slabs must be kept in a horizontal position and not stacked. Once cured, a release agent—such as talcum powder—may be applied to the stone surface to prevent the slabs from sticking together when stacked.

5. Cleaning

Use an appropriate cleaning agent to sanitize equipment before the adhesive cures.


AZ-1681 Epoxy Resin for Surface Crack Repair

AZ-1681 Epoxy Resin for Surface Crack Repair is a two-component epoxy adhesive system formulated for repairing irregular cracks, microfissures, porosity and surface defects in stone slabs. Supplied as components A and B, it cures to a strong, durable bond within the stone and is designed for the demands of natural stone processing and repair. A controlled mixing ratio of A:B = 4:1 gives repeatable results, and the cured resin delivers tensile shear strength of >=8 MPa.

Technical data: viscosity at 25 C is A 800-1200 / B 300-500 mPa.s. Gel time at 25 C is 15-25 min, with a curing time of 3-4 h. The low-viscosity formulation penetrates fine cracks and porous stone before hardening, which is essential for deep, uniform reinforcement. The cured resin is colorless and transparent where clarity matters for the finished stone appearance.

How it is applied: components A and B are mixed in the specified ratio, then poured or injected into the prepared crack, fissure or reinforcement zone. For vacuum infusion, the resin is drawn through flow media into the stone under vacuum. For surface repair, it is applied to fissures and allowed to cure before polishing. Correct mixing and pot life management are important for a complete cure.

Applications: repairing irregular cracks, microfissures, porosity and surface defects in stone slabs. The product is compatible with ANMYZ fiberglass mesh, vacuum bagging consumables and dispensing equipment for a complete working system.

Why choose ANMYZ: our epoxy resin range covers block coating, back netting, crack repair and luxury stone restoration, and our technical team can recommend the right formulation for your stone and process. Contact us for data sheets, packing sizes and pricing.

No comment

Product Detail

Mixing ratio: A:B = 4:1

Color: Colorless, transparent liquid.

Viscosity (25°C, mPa•s):

A: 800–1200

B: 300–500

Gel time (25°C, min): 15–25

Curing time (25°C, h): 3–4

Tensile shear strength (MPa): ≥8

Can be used for coating marble surfaces, repairing cracks and voids, and enhancing surface gloss after polishing.

250 kg/set

[Product Advantages]

1. High adhesion and strength; excellent penetration into small cracks;

2. Low odor; poses no health risks to workers;

3. Good resistance to aging and yellowing;

4. Compliant with GB18583 standards and RoHS directives; environmentally friendly.

[Instructions]

1. Slab Preparation

Slabs must be completely dry.

Remove any mud, oil, or other impurities from the slab surface.

2. Adhesive Preparation and Mixing

Mix the adhesive components in an A:B ratio of 4:1 (by weight) until homogeneous.

Use the adhesive within its pot life. The adhesive generates heat during the reaction; do not use it once the pot life has expired. A larger volume of mixed adhesive or a higher ambient temperature will result in a shorter pot life. If preparing a large batch, divide it promptly for use.

Do not swap the caps for components A and B. Keep the containers tightly closed at all times to prevent the ingress of moisture or dust from the air. It is recommended to use wide-mouthed containers for mixing to extend the adhesive's pot life.

3. Adhesive Application

Spread the adhesive evenly over the surface of the slab using a spatula, employing a back-and-forth motion. The recommended application rate is 80–150 g/m².

For cracks in the slabs, work the adhesive in using a back-and-forth motion to ensure complete penetration.

For larger defects (such as embedded soil or debris), remove the foreign material first; then, mix the adhesive with stone dust to perform the repair. Once cured, polish the area and reapply the adhesive. Do not use surface treatment agents that are not epoxy-based, as they may render the surface unsuitable for the application of epoxy adhesive.

4. Curing

The adhesive will reach an initial cure in 2 to 3 hours at room temperature (25 °C); the next processing stage can begin after 24 hours.

If possible, heat the stone (with the adhesive applied) to a temperature between 50 °C and 60 °C, and proceed with polishing after 2 to 3 hours.

Before the adhesive has cured, the stone slabs must be kept in a horizontal position and not stacked. Once cured, a release agent—such as talcum powder—may be applied to the stone surface to prevent the slabs from sticking together when stacked.

5. Cleaning

Use an appropriate cleaning agent to sanitize equipment before the adhesive cures.


Applications & Benefits

AZ-1681 Epoxy Resin for Surface Crack Repair

AZ-1681 Epoxy Resin for Surface Crack Repair is a two-component epoxy adhesive system formulated for repairing irregular cracks, microfissures, porosity and surface defects in stone slabs. Supplied as components A and B, it cures to a strong, durable bond within the stone and is designed for the demands of natural stone processing and repair. A controlled mixing ratio of A:B = 4:1 gives repeatable results, and the cured resin delivers tensile shear strength of >=8 MPa.

Technical data: viscosity at 25 C is A 800-1200 / B 300-500 mPa.s. Gel time at 25 C is 15-25 min, with a curing time of 3-4 h. The low-viscosity formulation penetrates fine cracks and porous stone before hardening, which is essential for deep, uniform reinforcement. The cured resin is colorless and transparent where clarity matters for the finished stone appearance.

How it is applied: components A and B are mixed in the specified ratio, then poured or injected into the prepared crack, fissure or reinforcement zone. For vacuum infusion, the resin is drawn through flow media into the stone under vacuum. For surface repair, it is applied to fissures and allowed to cure before polishing. Correct mixing and pot life management are important for a complete cure.

Applications: repairing irregular cracks, microfissures, porosity and surface defects in stone slabs. The product is compatible with ANMYZ fiberglass mesh, vacuum bagging consumables and dispensing equipment for a complete working system.

Why choose ANMYZ: our epoxy resin range covers block coating, back netting, crack repair and luxury stone restoration, and our technical team can recommend the right formulation for your stone and process. Contact us for data sheets, packing sizes and pricing.

AZ-1681 Stone adhesive/Epoxy resin for repairing surface cracks in stone slabs
Application:
The product is used to repair irregular fissures—such as micro-cracks (pinholes, "chicken-wire" patterns, or fine, winding cracks)—and uneven areas on the surface of various types of stone. It can serve as a replacement for the following products:
RESIN 5008 (used with catalysts BB25, BX30, or BX40)
RESIN 1006 (used with catalysts BB25, BX30, or BX40)
Long press to look detail
Long by picture save/share
INQUIRY

enquiry form:

  • Please enter the verification code

Inquiry Content:


You have no items to require

Add Successfully

AZ-1681 Stone adhesive/Epoxy resin for repairing surface cracks in stone slabs

enquiry
INQUIRY

enquiry form:

  • Please enter the verification code

Inquiry Content:


You have no items to require

Add Successfully

PRODUCTS

Epoxy Resin system for stones

Fiberglass mesh/woven

Abrasive

Diamond tools

 

 CONTACT

 

Tel: +852-59278153 
Tax:+852-59278153

Email : [email protected]

COMPANY

About   |  Production Ability    |   Our Advantages   |   Trade Capacity

 

PRODUCTS

Stone adhesive   |   Fiberglass mesh/woven

Abrasive   |   Vaccum Perfusion System

Copyright © 2015-2035 Anmyz Industry Ltd. All Rights Reserved. 

Phone
+86-15920009441
Working Time
Monday to Friday
Qrcode
Whatsapp
Add WeChat friend to learn more about the product
Use Enterprise WeChat
"Scan" to join the group chat
Copy success!
Add WeChat friend to learn more about the product
I see.